中文

ENGLISH

 
Tech & QA

Tech & QA

Vowin Material Specification And Capability

Process Stereolithography (SLA) Selective Laser Sintering(SLS)
Process Description SLA builds plastic parts a layer at a time using a laser to cure liquid photopolymer. SLA produces parts with very good dimensional accuracy and surface finish. Vowin employs master model makers to finish your SLA parts accurately to your 3D Data. Choices of materials are available to emulate a variety of thermo plastics. SLS uses a laser to trace over powder to selectively melt and bond the layers until the part is built. SLS builds parts in durable materials including Nylon and metals. A good choice for proto's that need to be tough.
Materials (see details on back) ABS-like: Somos 14120 PP-like: Accura 25 Clear: Accura 60 Nylon Nylon GF Wax Metals
Model Making Finish Standard: Support Removal & Bead Blast Engineering Review: Above + Wet Sanding Exterior Show Model: Master finish on exterior cosmetic area's High Show Model: Clear parts with interior+exterior polish
Secondary Finish Paint Texture Polish Semi-Clear Plating Metallic Artwork Threaded Inserts Paint Texture Polish Plating Metallic Artwork Threaded Inserts
PolyJet utilizes an inkjet that deposits photopolymer onto a build tray, the layers are cured by UV. PolyJet builds in super thin layers down to just 16 microns (0.0006 inch). Best for small parts with fine details. FDM extrudes material via a nozzle. The nozzle is mounted to a mechanical stage which can be moved in both horizontal and vertical directions. FDM builds parts in ABS and PC. Surface finish and accuracy is rougher than our other RP processes. The Rapid Casting process utilizes a master pattern to create a silicone rubber mold. Duplications are then cast in a vacuum chamber. Parts are very durable and cosmetically resemble injection molded parts. Vowin specializes in casting for Low Quantity Production, Over molded Parts, Lens, and Large Parts.
ABS-like TPE-like: Tango (Black or Gray) ABS Polycarbonate Wax ABS-like ABS/PC-like PP-like TPE-like Acrylic-like UL VO
Standard: Support Removal & Bead Blast Engineering Review: Above + Wet Sanding Exterior Show Model: Master finish on exterior cosmetic area's High Show Model: Clear parts with interior +exterior polish None Custom Molded-in: • Colors • Textures • Polish
Paint Texture Polish Semi-Clear Plating Metallic Artwork Threaded Inserts Paint Texture Plating Metallic Artwork Threaded Inserts Molded-in Color Molded-in Texture Rubber Overmolding Insert Molding High Polish Clear & Tints Metallic Paint & Plating Artwork Threaded Inserts

Prototyping Material Data Sheet

Rapid Prototyping Material Properties

Name Tensile Strength Notch lzod
SLA: PP-like 38 Mpa (5450-5570 PSI) 9-24J/m (0.4 ft-lb/in)
SLA: Clear 58-68 Mpa (8410-9860 PSI) 15-25J/m (0.3-05 ft-lb/in)
SLA: ABS-like 45.7 Mpa 23.5 J/m
SLS: Nylon 44 Mpa 8.5J/m
SLS: Nylon GF (Glass-Filled) 38.1 Mpa 602J/m
Objet: ABS-like 49.9 Mpa 37.5J/m
Objet: TPE-like (Elastomer) 2.0 NA
Heat Deflection/ Glass Transition Durometer
@66 PSI 58-63℃ (136-145°F) @264 PSI 51-55 ℃(124-131°F) Shore D 80
@66 PSI 53-55℃ (127-131°F) @264 PSI 48-50℃ (118-122°F) Shore D 86
@0.46 Mpa 53℃ Shore D 81
DTUL 0.45 Mpa ASTMD648: 177 °C NA
DTUL 0.45 Mpa ASTMD648: 175 °C NA
@66 PSI/264 PSI 120°F-49°C/ 113°F49°C Shore D 83
NA Shore A 61

Urethane Casting Rigid Material Data Sheet

Name Tensile Strength Notch lzod
UL-Rated 10650 PSI 1.6 ft. lbs/in
UL-Rated 10650 PSI 1.6 ft. lbs/in
PP-like Mpa 25 NA
ABS-like Mpa 70 kJ/m² 70
ABS/PC-like (High Temp) Mpa 61 kJ/m² 41
Acrylic-like / Tinted Mpa 75 charpy impact strength kJ/m² 27
Heat Deflection/ Glass Transition Durometer
@66 PSI 179° F Shore D1 85
55°C Shore D1 70
92°C Shore D1 82
T.M.A. Mettler 220°C Shore D1 80
HDT 1.8 Mpa 100°C Shore D1 87

Urethane Casting Elastomer Material Properties

Name Tensile Strength Notch lzod
TPE-like (30A - Elastomer) 675 PSI NA
TPE-like (40A - Elastomer) 65 PSI NA
TPE-like (50A - Elastomer) 845 Elasticity @100% strain 150 @200% strain 275 @300% strain 390 NA
TPE-like (60A - Elastomer) 685 Elasticity @100% strain 312 @200% strain 497 @300% strain 623 NA
TPE-like (80A - Elastomer) 1,900 NA
Heat Deflection/ Glass Transition Durometer
NA Shore A 32±2
NA Shore A 42±2
NA Shore A 50±2
NA Shore A 60±2
NA Shore A 80±2

Quality Assurance:

We have achieved ISO 9001:2000 Certirication. "Integrity Centered, Customer First, Quality Priority and Continuous Improvement" is our quality policy.

We have a complete set of standards for Prototype make, mold design, fabrication an inspection shich comply with the quality requirements of Europe,USA and Japan.

  • Competitive

  • One to One Service

  • Enginner Review

  • Quality

  • Fast Delivery

  • Request Quote Right Now

  • Design

    Prototype

    Low Volume Production

    Mold

    Production

    Contact